How lumber weight is calculated
Weight is simply the volume of wood times its density:
weight (lb) = actual thickness (in) × actual width (in) × length (in) ÷ 1,728 × density (lb/ft³) weight (kg) = thickness (m) × width (m) × length (m) × density (kg/m³)
Use the actual size, not the nominal one: a 2×4 is 1½″ × 3½″, so a 2×4×8 holds 1.5 × 3.5 × 96 ÷ 1,728 = 0.29 cubic feet of wood. At 33 lb/ft³ (dry Douglas fir) that is about 9.7 lb. The calculator uses the dressed sizes of the market you pick, so metric sizes such as 45 × 95 mm work the same way.
Density depends mostly on the species and on how much water is still in the wood. Densities here start from typical air-dry values (about 12% moisture) after the USDA Forest Products Laboratory Wood Handbook.
Lumber weight chart: pounds per foot
Weight per linear foot of common US sizes. SPF, Douglas fir and southern yellow pine are air-dry (about 12% moisture); pressure-treated (PT) pine is wet from the treating plant, which is how it usually comes off the rack. Multiply by the length in feet for one board.
| Size | SPF | Douglas fir | Southern pine | PT pine (wet) |
|---|---|---|---|---|
| 1×4 | 0.48 | 0.60 | 0.65 | 0.91 |
| 1×6 | 0.75 | 0.95 | 1.02 | 1.43 |
| 5/4×6 deck board | 1.00 | 1.26 | 1.36 | 1.91 |
| 2×4 | 0.96 | 1.21 | 1.30 | 1.82 |
| 2×6 | 1.50 | 1.90 | 2.04 | 2.86 |
| 2×8 | 1.98 | 2.50 | 2.69 | 3.77 |
| 2×10 | 2.53 | 3.19 | 3.43 | 4.81 |
| 2×12 | 3.07 | 3.88 | 4.17 | 5.85 |
| 4×4 | 2.23 | 2.81 | 3.03 | 4.25 |
| 4×6 | 3.51 | 4.42 | 4.76 | 6.68 |
| 6×6 | 5.51 | 6.95 | 7.48 | 10.49 |
Pounds per foot. Densities used: SPF 26 lb/ft³, Douglas fir 33, southern pine 36, wet PT pine 50.
Weight of common boards
| Board | SPF | Douglas fir | Southern pine | PT pine (wet) |
|---|---|---|---|---|
| 2×4 × 8 ft | 7.6 lb | 9.7 lb | 10.4 lb | 14.6 lb |
| 2×6 × 8 ft | 12.0 lb | 15.2 lb | 16.3 lb | 22.9 lb |
| 2×10 × 16 ft | 40.4 lb | 51.0 lb | 54.9 lb | 77.0 lb |
| 2×12 × 16 ft | 49.2 lb | 62.0 lb | 66.7 lb | 93.6 lb |
| 4×4 × 8 ft | 17.8 lb | 22.5 lb | 24.2 lb | 34.0 lb |
| 6×6 × 8 ft | 44.1 lb | 55.6 lb | 59.8 lb | 83.9 lb |
Green, air-dry and kiln-dried weight
Freshly sawn (“green”) wood can hold as much water as wood fibre, so it is far heavier than dry lumber. The calculator handles moisture like this:
- Kiln-dried: softwood framing lumber stamped KD-19 is dried to 19% moisture or less and usually ships near 15%; kiln-dried hardwood is dried to about 7%. Below about 30% moisture, weight changes in step with the water, so density ≈ air-dry density × (1 + moisture) ÷ 1.12. Kiln-dried SPF comes out about 3% heavier than air-dry; kiln-dried oak about 4% lighter.
- Air-dry (12%): the reference densities, typical of lumber that has sat indoors for a while.
- Green: air-dry density times a green factor taken from the Wood Handbook green vs air-dry weights where the species matches — Douglas fir 43 vs 34 lb/ft³ (×1.26), western hemlock for hem-fir (×1.32), Engelmann spruce for spruce and SPF (×1.33), western red cedar (×1.17), redwood (×1.79). Other species use a typical ×1.4. Green weight varies a lot between boards, so treat it as a rough figure.
These are estimates. A moisture meter and a bathroom scale on one board will always beat any chart.
How much does pressure-treated lumber weigh?
Pressure-treated pine is soaked with a waterborne preservative under pressure, and it usually leaves the plant wet. That is why a treated 2×4 feels so much heavier than an untreated one. The calculator uses about 50 lb/ft³ (800 kg/m³) for wet treated southern pine — roughly 40% heavier than the same board dry. A wet PT 2×4×8 weighs about 14–15 lb and a 6×6×8 post about 84 lb.
Treated lumber loses that water over weeks or months in the open. Choose Air-dry or Kiln-dried for KDAT (kiln-dried after treatment) lumber or for boards that have dried out; the calculator then uses the untreated species density.
Hauling lumber: pickup loads
A common rule of thumb is that a ½-ton pickup carries about 1,000–1,500 lb of payload, but the real figure depends on the truck and its options — check the tire and loading sticker on the driver’s door jamb, and remember that passengers count toward payload. The calculator shows your load as a share of 1,500 lb and warns when it is more.
For scale: fifty 2×4×8 SPF studs weigh about 380 lb, but fifty wet PT 2×6×12s weigh about 1,700 lb — already more than many half-ton trucks should carry. For larger orders, ask the yard to deliver. To see what an order costs, use the MBF price calculator; for board feet, the board foot calculator.
Frequently asked questions
How much does a 2×4 weigh?
A kiln-dried 2×4×8 weighs about 8 lb in SPF, about 10 lb in Douglas fir and 10–11 lb in southern yellow pine. A wet pressure-treated 2×4×8 weighs about 14–15 lb.
How much does a 2×10 weigh?
A 2×10 weighs about 2.5–3.4 lb per foot dry, depending on species, so a 2×10×16 is roughly 40 lb in SPF and 55 lb in southern pine. Wet treated, it is about 77 lb.
How much does pressure-treated lumber weigh?
Wet from the plant, treated pine weighs about 50 lb per cubic foot — about 1.8 lb per foot for a 2×4 and 2.9 lb per foot for a 2×6. It gets lighter as it dries.
Is green lumber heavier than kiln-dried?
Yes. Green Douglas fir weighs about 43 lb per cubic foot against 34 lb air-dry, according to Wood Handbook figures — about 26% more. Some species, like redwood, are nearly twice as heavy green.
How much lumber can a half-ton pickup carry?
Rule of thumb: 1,000–1,500 lb of payload, including passengers — check your door-jamb sticker. That is roughly 130–190 kiln-dried 2×4×8 SPF studs, or 70–100 wet PT 2×4×8s.
How much does a board foot of lumber weigh?
An actual board foot (144 cubic inches) weighs density ÷ 12: about 2.2 lb for SPF, 2.8 lb for Douglas fir, 3.0 lb for southern pine and 4.2 lb for wet treated pine.